Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 104R PC (Europe-Africa-Middle East) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informat.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 201R PC (Europe-Africa-Middle East) LEXAN 201R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD104R PC FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East) Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS7R PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ4820 PC (Europe-Africa-Middle East) LEXAN OQ4820 is a high viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard resins. Fields of application for this material are optical lenses, f.i. in sun glass.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Asia Pacific) Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 955U PC (Europe-Africa-Middle East) Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179 |
Chi Mei Wonderlite® PC-110L Polycarbonate - UV Stabilized Head Lamp |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati.. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SD1318 PC High viscosity, UV stabilized multi purpose grade. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B1X25 HI PA6 High Impact Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP4EU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Charpy Impact, Notched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS6R PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable... |