Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Filler Content 10 %
10 %
±2%; Polykemi
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 54

@Time 15.0 sec
54

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 19.0 MPa
<= 2760 psi
ISO/R527
Elongation at Yield 8.0 %
8.0 %
ISO/R527
Flexural Strength <= 25.0 MPa
<= 3630 psi
ISO 178
Flexural Modulus 1.30 GPa

@Temperature 23.0 °C
189 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched 1.50 J/cm²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
120°C/h; ISO 75/1
Vicat Softening Point 132 °C

@Load 1.00 kg
270 °F

@Load 2.21 lb
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Mold Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Injection Pressure 90.0 - 110 MPa
13100 - 16000 psi
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Speed () High
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved