Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 230 °C |
12 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE HJ-75 UV1 Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 141 PC (Europe-Africa-Middle East) LEXAN 141 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 920A PC (Europe-Africa-Middle East) LEXAN 920A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® AD143 PC LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 144H PC (Europe-Africa-Middle East) LEXAN 144H resin is a medium viscosity multi purpose product with ease of processing. It is intended for FDA food contact applications with limited color options. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP3REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 260 °C |
12 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East) LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 340 °C |
12 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 360 °C |
12 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 360 °C |
12 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Melt Index of Compound | 12 - 14 g/10 min | 12 - 14 g/10 min | I Preparation |
Sibur ABS 2020-32 Molding Grade ABS Plastic Thermal, light and atmospheric resistant with high fluidity for technical articles and parts of automobile building. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Melt Index of Compound | 12 - 20 g/10 min | 12 - 20 g/10 min | |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow H700-12 Polypropylene Homopolymer Resin Complies withU.S. FDA 21 CFR 177.1520 (c) 1.1FDA-DMFUnderwriters Laboratories Inc.Europe EU-Directive 2002/72/ECLondon Metal Exchange - Part 6B Rules - PolypropyleneCanadian HPFB No ObjectionDOW H70.. |
|||
Melt Index of Compound | 12 g/10 min | 12 g/10 min | ASTM D1238 |
Cheng Yu Plastic E500G20 PC/PET, 20% Glass Fiber |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
A.D. Compound Adene NCFAG Copolymer 20% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 265 °C |
12 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
3M Dyneon™ THV 815GZ Fluorothermoplastic Granules Dyneon THV 815 GZ provides a balance of low permeation, thermal stability, and melt processability. IT can be used to prepare molded parts and extruded films, tubes, profiles, and wire coatings. It .. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |