Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 0.500 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.300 - 0.500 MPa
43.5 - 72.5 psi
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 T10 Thermoplastic Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Copyright © lookpolymers.com All Rights Reserved