Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.80 J/cm² @Temperature -20.0 °C |
13.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYelast TPE R44 T10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in.. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev.. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eA |
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 0.000 °C |
13.3 ft-lb/in² @Temperature 32.0 °F |
ISO R179 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |