Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.30 GPa | 189 ksi | |
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Flexural Modulus | >= 1.30 GPa | >= 189 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol R120MK Polypropylene REPOL Polypropylene R120MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet COPYLENE™ CH003T, a fractional melt flow polypropylene homopolymer resin, is available in pellet form. Replacement alternative for Pro-fax® HL561CInformation provided by Phillips 66. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat Primary Processing Method: Injection MoldingKey Features: nucleated and antistatic, high flow polypropylene homopolymer resin, FDA acceptable, short cycle time for high productivity, resists dust pi.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 2300NC Polypropylene Block Copolymer CHARACTERISTICS: MEDIUM FLOW, GOOD IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, FURNITURES, CRATES |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 2363LC Polypropylene Block Copolymer CHARACTERISTICS: CONTAIN UV STABILIZER ADDITIVE, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES, FURNITURES, CRATES |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | DIN 53452; ASTM D790 |
Kolon Kopa® KN151 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 A |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ TKS708D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS708D medium high melt flow, 1,300 MPa flexural modulus, UV-stabilized, high impact thermoplastic elastomeric olefin (TEO) resin has an excellent combination of propert.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FD000 PE LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Lubrizol Isoplast® 301 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene ATOFINA Polypropylene MR 2001 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene ATOFINA Polypropylene MR 2002 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Eastman Tenite 572E3720012 Cellulose Acetate Butyrate, Clear, Trsp Applications:FilmsProfilesSheetProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a wa.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, Conditioned Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Borealis HD214CF Polypropylene Homopolymer HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus.. |
|||
Flexural Modulus | 1.30 - 3.70 GPa | 189 - 537 ksi | Average value: 2.81 GPa Grade Count:45 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 80x10x4 mm specimen, 2 mm/min; ASTM D790 |
LyondellBasell INDURE™ X210 TPO Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Appli.. |