Material Notes:
The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant HC compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.021 cm/cm

@Thickness 3.18 mm
0.021 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.036 cm/cm

@Thickness 3.18 mm
0.036 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 77.0 MPa
11200 psi
ISO 527-2
Flexural Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/3A
Thermal Properties Metric English Comments
Melting Point 255 - 265 °C
491 - 509 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
Unannealed; ISO 75-2/A
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 270 °C
482 - 518 °F
Middle Barrel Temperature 260 - 280 °C
500 - 536 °F
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Nozzle Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Descriptive Properties Value Comments
Additive Lubricant
Appearance Natural Color
Features Good Chemical Resistance
Good Colorability
Lubricated
Medium Impact Resistance
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Hospital Goods
Housings
Medical Appliances
Medical/Healthcare Applications
Users viewing this material also viewed the following: