Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)
(Unverified Data**) Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**) Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface .. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Conditioned) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Rear Barrel Temperature | 250 °C | 482 °F | |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 1 |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Rear Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Compression Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |