Polymer Property : Front Barrel Temperature = 554 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Zone
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Start Point: 280°C
Kingfa JH720 G30 30% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact
Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID HM2604AW PA6+GF60%
Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Injection Molding
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface
Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY
Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This ..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber
Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica..
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Solvay TECHNYL® A 216 PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced
Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as beari..
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY
Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® 27010ST PA66, DRY
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Zone 3
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Zone 3
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded
AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Zone
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM  (discontinued **)<
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)  (discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..