Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 255 - 265 °C | 491 - 509 °F | ASTM D789 |
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66) The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah.. |
|||
Melting Point | 255 - 265 °C | 491 - 509 °F | ASTM D789 |
PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66) The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g.. |
|||
Melting Point | 238 - 265 °C | 460 - 509 °F | Average value: 255 °C Grade Count:14 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Melting Point | 254 - 265 °C | 489 - 509 °F | Average value: 258 °C Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Melting Point | 254 - 265 °C | 489 - 509 °F | Average value: 258 °C Grade Count:43 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melting Point | 221 - 265 °C | 430 - 509 °F | Average value: 256 °C Grade Count:11 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Melting Point | 255 - 265 °C | 491 - 509 °F | Average value: 259 °C Grade Count:7 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 254 - 265 °C | 490 - 509 °F | Average value: 259 °C Grade Count:30 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Melting Point | 250 - 265 °C | 482 - 509 °F | ASTM D789 |
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 250 - 265 °C | 482 - 509 °F | ASTM D789 |
Lucent Polymers 66-41 Nylon 66, Toughened Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 250 - 265 °C | 482 - 509 °F | ASTM D789 |
Lucent Polymers G66-13 Nylon 66, 13% Glass Fiber Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 250 - 265 °C | 482 - 509 °F | ASTM D789 |
Lucent Polymers G66-33 Nylon 66, 33% Glass Fiber Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 255 - 265 °C | 491 - 509 °F | ISO 3146-A |
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 260 - 265 °C | 500 - 509 °F | |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 215 - 265 °C | 419 - 509 °F | Average value: 221 °C Grade Count:67 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |