Material Notes:
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Key Featurs:Recommended for applications requiring excellent flex fatigue resistance.Recommended for applications requiring excellent ozone resistance.Designed for improved UV resistance.Compliant to EU Directive 2003/11/EC regarding marketing and use of certain dangerous substances and preparations, specifically pentabromodiphenyl ether or octabromodiphenyl ether.Applications:Automotive- Weather Seals, Seals and GasketsUses:Automotive ApplicationsAutomotive Exterior TrimProcessing Method: Coextrusion, Profile Extrusion, Thermoforming, Extrusion, Sheet Extrusion and Vacuum Forming Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86

@Thickness 2.00 mm,
Time 15.0 sec
86

@Thickness 0.0787 in,
Time 0.00417 hour
ISO 868
Tensile Strength at Break 9.58 MPa
1390 psi
Across Flow; ASTM D412
Tensile Stress 4.60 MPa

@Strain 100 %
667 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 460 %
460 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 87
Color Black
Form Pellets