Axiall 15641 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 15641 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-rigid, fungus and microbe resistant insulation compound recommended for UL Style #1061 and CSA-SR applications. The compound has good migration and toner resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 63
57 - 63
delayed; ASTM D-2240
Tensile Strength, Yield 23.1 MPa
3350 psi
ASTM D-638
Elongation at Yield 276.3 %
276.3 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.02051 GPa
2.975 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -8.00 °C
17.6 °F
ASTM D-746
Oxygen Index 28 %
28 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 196 °C
385 °F