Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Density 0.815 g/cc
0.0294 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Hardness, Shore D 79
79
15 sec; ASTM D2240
82
82
ASTM D2240
Tensile Strength, Yield 48.9 MPa
7090 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 86.9 MPa
12600 psi
ASTM D790
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Vicat Softening Point 81.0 °C
178 °F
Processing Properties Metric English Comments
Mold Temperature 193 - 207 °C
379 - 405 °F
Blow Molding
Descriptive Properties Value Comments
Features General Purpose
High Gloss
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose
Packaging
Sheet