Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP212VO Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | DIN 53452; ASTM D790 |
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN1322VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 3.04 GPa @Thickness 6.40 mm |
441 ksi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Flexural Modulus | 3.04 GPa @Thickness 3.20 mm |
441 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN133G8ST Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 3.04 GPa @Thickness 3.20 mm |
441 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | |
Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 3.04 GPa @Thickness 3.20 mm |
441 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 206 General Purpose Polystyrene CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Flexural Modulus | 3.04 GPa @Temperature 120 °C |
441 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 6010FGN Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 3.04 GPa | 441 ksi | ASTM D790 |
Samyang Trilen® 9550T30 Polypropylene, Reinforced Mechanical strength and thermal resistance are excellent.9550T30 is a non-flame retardant, reinforced grade.Information provided by Samyang. |