Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable Y152 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D-792 |
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R246AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
RTP Company RTP 1300 AR 15 Polyphenylene Sulfide (PPS) Aramid Fiber 15%
(discontinued **)& Aramid Fiber 15%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Specific Gravity | 1.37 g/cc @Temperature 23.0 °C |
1.37 g/cc @Temperature 73.4 °F |
Crystalline; ISO 1183 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Teknor Apex APEX® CX 2001-73 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Teknor Apex APEX® 84132UV Polyvinyl Chloride Compound Notes: Sunlight Resistant Tray Cable Coax Jacket Temperature Rating: 80°CInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SRF 3704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D 792 |
RTP Company RTP 1400 A-300 Polyethersulfone (PES), UL94 V-0 |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D 792 |
RTP Company RTP 2200 HF TFE 15 Polyetheretherketone (PEEK), PTFE Lubricated - High Flow |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | |
Epoxy Technology EPO-TEK® TZ101 Thermally Conductive Epoxy Product Description: EPO-TEK® TZ101 is a single component, electrically insulating, thermally conductive epoxy adhesive designed for heatsinking of semiconductors, hybrids, electronics, and optics... |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Colorite Polymers CS1537SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D790 |
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | Part A; TM R050-16 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Specific Gravity | 1.37 g/cc | 1.37 g/cc | ISO 1183 |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |