Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.815 g/cc | 0.0294 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Density | 0.815 - 0.862 g/cc | 0.0294 - 0.0311 lb/in³ | |
Lord Adhesives Chemlok® 5151 Adhesive Chemlok® 5151 is a single coat adhesive used to bond fluorocarbon based elastomers to metal. It is particularly effective on phosphate coated metals. Chemlok 5151 adhesive will bond a wide variet.. |
|||
Density | 0.815 g/cc @Temperature 15.6 °C |
0.0294 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Isopar™ V Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europ.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
BASF Diethyl Ketone Formula: C5H10OCAS: 96-22-0Description: Dichlorohexane is a colorless to yellowish liquid with an aromatic odor. Synonyms: Pentan-3-on, 3-Pentanone, DEK, Diethyl KetoneApplications: Intermediate use.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
BASF Pentanol Formula: C5H12OCAS: 71-41-0Description: Pentanol is a colorless liquid with an offensive odor.Synonyms: Pentan-1-ol, 1-Pentanol, n-Amyl alcoholApplications: Intermediate used in the production of Co.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
BASF Pentanol Mixture Formula: C5H12OCAS: 94624-12-1Description: Pentanol mixture is a colorless to yellow liquid, with a sweetish odor. It is soluble in water and with many organic solvents.Applications: Intermediate u.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
3M Scotch-Weld™ Hi-Strength Laminating 92 Cylinder Spray Adhesive A high performance, high temperature resistant, tack industrial grade spray adhesive designed for use in a wide variety of applications.Features:It can be used for high pressure laminate, veneers, f.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
3M 2262T Adhesion Promoter 3M Adhesion Promoter 2262T is a ready-to-use, pre-diluted (10 MEK/1 part 2262) version of 3M Scotch-Grip Plastic Adhesive 2262. It is a liquid primer intended for most flexible and rigid PVC compoun.. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
3M Multi-purpose 27 Spray Adhesive A versatile, economical, industrial grade, mist spray aerosol adhesive.Features:Extremely versatile adhesive for lightweight applicationsFast tacking mist spray adhesive with very little soak in on .. |
|||
Density | 0.815 g/cc | 0.0294 lb/in³ | |
3M 06396 Adhesion Promoter 3M Adhesion Promoter 06396 is a liquid primer used to improve the adhesion of 3M Automotive Attachment Tapes to most low surface energy plastic materials as well as injection-molded body side moldin.. |