Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.45 %

@Time 86400 sec
0.45 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 193 MPa
28000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 276 MPa
40000 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm

@Thickness 3.17 mm
3.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 13.9 J/cm

@Thickness 3.17 mm
26.0 ft-lb/in

@Thickness 0.125 in
ASTM D256