Mechanical Properties Metric English Comments
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid)
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by..
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Tensile Modulus 2.79 GPa
405 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Tensile Modulus 2.79 GPa
405 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Tensile Modulus 2.79 GPa
405 ksi
ASTM D638
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Modulus 2.79 GPa
405 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings 211 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.79 GPa
405 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66
LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant.
Tensile Modulus 2.79 GPa
405 ksi
ASTM D638
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame..
Tensile Modulus 2.79 GPa
405 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Tensile Modulus 2.79 GPa
405 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI
LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated.
Tensile Modulus 2.79 GPa
405 ksi
ASTM D638
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r..
Copyright © lookpolymers.com All Rights Reserved