Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 441 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid)
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Flexural Modulus 3.04 GPa
441 ksi
DIN 53452; ASTM D790
Kolon SPESIN® KP212VO Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Modulus 3.04 GPa
441 ksi
DIN 53452; ASTM D790
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Flexural Modulus 3.04 GPa
441 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN1322VO Flame Retardant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 3.04 GPa

@Thickness 6.40 mm
441 ksi

@Thickness 0.252 in
2.8mm/min; ASTM D790
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
Flexural Modulus 3.04 GPa

@Thickness 3.20 mm
441 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY SC3154 PC+GF15%
Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide..
Flexural Modulus 3.04 GPa
441 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN133G8ST Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 3.04 GPa

@Thickness 3.20 mm
441 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9..
Flexural Modulus 3.04 GPa
441 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66
LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 3.04 GPa
441 ksi
Shinil Chemical SHINFLAME PBT Flame Retardant Polymer Connector
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..
Flexural Modulus 3.04 GPa

@Thickness 3.20 mm
441 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SC 206 General Purpose Polystyrene
CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,..
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS ..
Flexural Modulus 3.04 GPa

@Temperature 120 °C
441 ksi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Flexural Modulus 3.04 GPa
441 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 6010FGN Nylon 66
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Flexural Modulus 3.04 GPa
441 ksi
ASTM D790
Samyang Trilen® 9550T30 Polypropylene, Reinforced
Mechanical strength and thermal resistance are excellent.9550T30 is a non-flame retardant, reinforced grade.Information provided by Samyang.
Copyright © lookpolymers.com All Rights Reserved