PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.014 - 0.022 cm/cm
0.014 - 0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.8 MPa
7800 psi
ASTM D638
Elongation at Break 24 %
24 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.47 GPa
503 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C

@Thickness 3.18 mm
163 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 277 - 299 °C
531 - 570 °F
Mold Temperature 82.2 - 104 °C
180 - 219 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Filler / Reinforcement Mineral Filler, 35% Filler by Weight
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications