Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 152 MPa
22000 psi
ASTM D-638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D-638
Tensile Modulus 7.586 GPa
1100 ksi
ASTM D-638
Flexural Strength 255 MPa
37000 psi
ASTM D-790
Flexural Modulus 7.586 GPa
1100 ksi
ASTM D-790
Izod Impact, Notched 3.63 J/cm
6.80 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 13.35 J/cm
25.01 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D-648
Processing Properties Metric English Comments
Rear Barrel Temperature 204 - 227 °C
400 - 440 °F
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
Front Barrel Temperature 216 - 238 °C
420 - 460 °F
Nozzle Temperature 221 - 243 °C
430 - 470 °F
Melt Temperature 216 - 238 °C
420 - 460 °F
Mold Temperature 87.8 °C
190 °F
Injection Velocity 50.8 - 76.2 mm/sec
2.00 - 3.00 in/sec
Drying Temperature 88.0 °C

@Time 14400 sec
190 °F

@Time 4.00 hour
Moisture Content <= 0.020 %
<= 0.020 %
Back Pressure 0.172 - 0.345 MPa
25.0 - 50.0 psi
Cushion 0.635 cm
0.250 in
Screw Speed 30 - 50 rpm
30 - 50 rpm
Descriptive Properties Value Comments
Injection Pressure Medium to maximum