Advanced Polymer Alloys DuraGrip™ 6140 TR Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ 6140 TR Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® DGR6140TR is a translucent thermoplastic elastomer formulated for excellent elastic properties and enhanced adhesion to various engineered thermoplastics using insert molding, co-injection molding and co-extrusion processes. 6140TR bonds tenaciously to polycarbonate, polycarbonate alloys, ABS, ASA, acrylics, and cellulosic materials. It will also bond to various nylons and PET. DuraGrip 6140TR is hygroscopic and drying is recommended at 150F for 3 to 4 hours to ensure optimum aesthetics, properties and adhesion.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 0.994 g/cc
0.994 g/cc
ASTM D471
Viscosity 266000 cP

@Shear Rate 294 1/s,
Temperature 190 °C
266000 cP

@Shear Rate 294 1/s,
Temperature 374 °F
ASTM D3835
Melt Index of Compound 12.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
12.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
5 Sec; ASTM D2240
Tensile Strength at Break 7.894 MPa
1145 psi
ASTM D412
Elongation at Break 647 %
647 %
ASTM D412
100% Modulus 0.00123 GPa
0.178 ksi
ASTM D412
300% Modulus 0.00250 GPa
0.362 ksi
ASTM D412
Graves Tear Strength 23.7 kN/m

@Temperature 24.0 °C
135 pli

@Temperature 75.2 °F
Die C; ASTM D624
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F