Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401, Nylon 6 Injection molding grade. Dry As Molded. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minima.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401, Nylon 6, at 50% Relative Humidity Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 402 Nylon 6 Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 404 Nylon 6, 50% RH Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406 Nylon 6 Injection molding grade. Dry as molded. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded f.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406F Nylon 6 Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 469 °F | |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Nozzle Temperature | 204 - 243 °C | 399 - 469 °F | |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 470 °F | |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 470 °F | |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 232 - 243 °C | 450 - 470 °F | |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 469 °F | Average value: 231 °C Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Nozzle Temperature | 54.4 - 243 °C | 130 - 470 °F | Average value: 220 °C Grade Count:27 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |