Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Nozzle Temperature | 221 °C | 430 °F | Extrusion |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 221 - 249 °C | 430 - 480 °F | Average value: 238 °C Grade Count:8 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Nozzle Temperature | 221 - 232 °C | 430 - 450 °F | |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |