Polymer Property : Rear Barrel Temperature = 400 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White
Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural
Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 227 °C
400 - 440 °F
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas..
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 227 °C
400 - 440 °F
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel
Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 204 - 221 °C
400 - 430 °F
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 204 - 238 °C
400 - 460 °F
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 204 - 238 °C
400 - 460 °F
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded
Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 204 - 216 °C
400 - 420 °F
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled
X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc..
Rear Barrel Temperature 204 - 216 °C
400 - 420 °F
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled
X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn ..
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
Rear Barrel Temperature 204 - 221 °C
400 - 430 °F
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel a..
Rear Barrel Temperature 204 - 221 °C
400 - 430 °F
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer
DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent soft touch feel a..
Rear Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.