Polymer Property : Nozzle Temperature = 430 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black
Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White
Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade
Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural
Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In..
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas..
Nozzle Temperature 221 - 243 °C
430 - 470 °F
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas..
Nozzle Temperature 221 - 229 °C
430 - 445 °F
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Nozzle Temperature 221 - 229 °C
430 - 445 °F
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Nozzle Temperature 221 - 271 °C
430 - 520 °F
Diamond Polymers ASA S710
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Nozzle Temperature 221 - 271 °C
430 - 520 °F
Diamond Polymers ASA T-120
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 221 - 232 °C
430 - 450 °F
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.