Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibrations, water, gases, oils, hydrocarbons and many chemicals.Applications:Ideal to fill gaps up to 0.008”Excellent for press and slip fitting parts that need to be disassembled.Withstands working temperatures up to 300ºFRetaining sleeves, pulleys, gears, rotors and fans on shafts.Mounting sleeves, securing bushings, bearings and plugs in housing.Excellent retaining and sealing compoundPart Numbers for this data: 17-001-ED, 17-010-ED, 17-050-ED, 17-250-ED, 17-1000-EDInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Brookfield Viscosity 1000 cP
1000 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 12.0 MPa

@Temperature 22.0 °C,
Time 86400 sec
>= 1740 psi

@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
>= 16.0 MPa

@Temperature 22.0 °C,
Time 108000 sec
>= 2320 psi

@Temperature 71.6 °F,
Time 30.0 hour
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 37.8 °C
>= 100 °F
Processing Properties Metric English Comments
Cure Time 120 - 180 min
2.00 - 3.00 hour
Functional
1440 min
24.0 hour
Full
30.0 min

@Temperature -55.0 - 150 °C
0.500 hour

@Temperature -67.0 - 302 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Yellow
Chemical Resistance 100% Initial Strength Retained
Acetone at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
100% Initial Strength Retained
Acetone at 22°C, at 1000hrs
100% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
95% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
Composition Methacrylate Esters
Gap Fill 0.008"