Polymer Property : Shear Strength = 2320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 16.0 MPa

@Temperature 22.0 °C,
Time 108000 sec
>= 2320 psi

@Temperature 71.6 °F,
Time 30.0 hour
ISO 10123; Compressive, Steel pins and collars
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration..
Shear Strength 16.0 MPa

@Temperature 149 °C
2320 psi

@Temperature 300 °F
Lap Shear
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.06 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Shear Strength 16.0 MPa

@Temperature 149 °C
2320 psi

@Temperature 300 °F
Lap Shear
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Shear Strength 16.0 MPa

@Temperature 177 °C
2320 psi

@Temperature 351 °F
Short Beam
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel