Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor .. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 65 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 75 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings with lubricating properties to facilitate proper assembl.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT TURBO SEAL SERIES 80 is a high performance control strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings.NSF Certified Certified to ANSI/NSF Sta.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 85 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound preven.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 95 is a medium strength high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absenc.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 11 Anaerobic Thread Locking Compound TURBO-LOCK 11 SERIES is a fast curing, BLUE, removable, medium strength, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibration.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 11-HT Anaerobic Thread Locking Compound TURBO-LOCK 11-HT SERIES is a fast curing, BLUE, removable, medium strength, high temperature, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibr.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 11-OR Anaerobic Thread Locking Compound TURBO-LOCK 11-OR SERIES is a fast curing, BLUE, removable, medium strength, oil resistant, primerless, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 12 Anaerobic Thread Locking Compound TURBO-LOCK 12 SERIES is a fast curing, medium to high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water,.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 13 Anaerobic Thread Locking Compound TURBO-LOCK 13 SERIES is a RED, high temperature, high strength, permanent, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many c.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 14 Anaerobic Thread Locking Compound TURBO-LOCK 14 SERIES is a fast curing, high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oi.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | Average value: 0.300 J/g-°C Grade Count:20 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 16 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 16 is a fast curing, GREEN, medium strength, wicking grade, anaerobic thread-locking compound for bonding and sealing threads, and pre-assembled parts. It is highly resistance to h.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 17-HT Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-HT is a fast curing, GREEN, high temperature, high strength, high viscosity, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical p.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Palm Labs Adhesives TURBO-LOCK SERIES 17-OR Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-OR is a fast curing, GREEN, high strength, oil resistant, close fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly .. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | A Instruments Model 2920 modulated DSC, ASTM TM E1269. |
DuPont™ Nomex® 430 1200 Denier Aramid Yarn A high crystallinity natural filament yarn of NOMEX with higher strength and chemical resistance than staple spun yarns. Type 430 is used where the aesthetics and properties of a filament yarn are .. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | A Instruments Model 2920 modulated DSC, ASTM TM E1269. |
DuPont™ Nomex® 450 Aramid Staple Fiber A natural staple fiber. It has higher crystallinity and strength than Type 455 and 462 fibers, and is sold as a 100% meta-aramid staple in various cut lengths. It is used in applications requiring.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Specific Heat Capacity | 0.300 J/g-°C | 0.0717 BTU/lb-°F | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |