Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 16.0 MPa @Temperature 22.0 °C, Time 108000 sec |
>= 2320 psi @Temperature 71.6 °F, Time 30.0 hour |
ISO 10123; Compressive, Steel pins and collars |
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration.. |
|||
Shear Strength | 16.0 MPa @Temperature 149 °C |
2320 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.06 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 16.0 MPa @Temperature 149 °C |
2320 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 16.0 MPa @Temperature 177 °C |
2320 psi @Temperature 351 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |