Thermal Properties Metric English Comments
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT
TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT
TURBO SEAL SERIES 65 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT
TURBO SEAL SERIES 75 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings with lubricating properties to facilitate proper assembl..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT
TURBO SEAL SERIES 80 is a high performance control strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings.NSF Certified Certified to ANSI/NSF Sta..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT
TURBO SEAL SERIES 85 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound preven..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT
TURBO SEAL SERIES 95 is a medium strength high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absenc..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound
TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 11 Anaerobic Thread Locking Compound
TURBO-LOCK 11 SERIES is a fast curing, BLUE, removable, medium strength, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibration..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 11-HT Anaerobic Thread Locking Compound
TURBO-LOCK 11-HT SERIES is a fast curing, BLUE, removable, medium strength, high temperature, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibr..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 11-OR Anaerobic Thread Locking Compound
TURBO-LOCK 11-OR SERIES is a fast curing, BLUE, removable, medium strength, oil resistant, primerless, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 14 Anaerobic Thread Locking Compound
TURBO-LOCK 14 SERIES is a fast curing, high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oi..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound
TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat..
Flash Point >= 37.8 °C
>= 100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration..
Flash Point 37.8 °C
100 °F
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl..
Flash Point >= 37.8 °C
>= 100 °F
ASTM D56
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
Flash Point >= 37.8 °C
>= 100 °F
ASTM D56
Humiseal 1C65 Silicone Conformal Coating
Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Copyright © lookpolymers.com All Rights Reserved