Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1000 cP | 1000 cP | 60 rpm; ISO 1652 |
Polimeri Europa Intex® 131 Styrene - Butadiene Copolymer Intex® 131 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain an.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | 60 rpm; ISO 1652 |
Polimeri Europa Intex® 132 Styrene - Butadiene Copolymer Intex® 132 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain an.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | 60 rpm; ISO 1652 |
Polimeri Europa Intex® 2720 Styrene - Butadiene Copolymer Intex® 2720 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain a.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | 60 rpm; ISO 1652 |
Polimeri Europa Intex® 2740 Styrene - Butadiene Copolymer Intex® 2740 is an aqueous anionic dispersion of a styrene-butadiene copolymer with high solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain a.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | #20/200 |
Mallard Creek Polymers BarrierPro® 4551 Styrene-Butadiene Emulsion Barrier Pro® 4551 is a carboxylated styrene-butadiene emulsion with excellent strength properties, high resistance to liquid water and water vapor, high blush resistance and excellent adhesion to.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | #20/200 |
Mallard Creek Polymers Rovene® 6112 Resin Supported Emulsion Rovene® 6112 is a hard, film forming, low glycol ether and VOC vehicle with a moderately low glass transition temperature for flexographic and gravure inks and overprint varnishes. Rovene® 611.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | #20/200 |
Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard subs.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | #20/200 |
Mallard Creek Polymers Rovene® 8001 Hybrid Styrene-Butadiene Emulsion Rovene® 8001 is a hybrid of natural binder and self crosslinking carboxylated styrene-butadiene emulsion developed especially for use on organic spunbond roofing mats where it imparts excellent t.. |
|||
Brookfield Viscosity | 1000 - 5000 cP | 1000 - 5000 cP | DOP 60phr; ASTM D1824 |
LG Chemical PB1752 PVC General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Hydrosize® U1-03 Phenoxy modified polyurethane dispersion Description: Phenoxy modified polyurethane dispersionUsage: Hydrosize® U1-03 is designed to be a fiber sizing coating with excellent adhesion and abrasion resistanceInformation provided by Michel.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 91840 Nonionic HD polyethylene / paraffin wax emulsion Description: Nonionic HD polyethylene / paraffin wax emulsionUsage: Michem® Emulsion 91840 is a wax emulsion that provides superior rub resistance and gloss when used as an additive in overprint .. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Lube 270R Anionic paraffin/polyethylene wax emulsion Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Lube 270R is an additive which provides excellent water resistance in paint and coating formulations. This product is useful .. |
|||
Brookfield Viscosity | 1000 - 4000 cP | 1000 - 4000 cP | Spindle # 3, rpm 30 |
Michelman® Michem® Prime 4983-40R Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 498340R is a high solids, more economical version of Michem® Prime 4983R. Like Michem® Prime 4983R, this product provides o.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Shield 422 Anionic dispersion of polyethylene wax Description: Anionic dispersion of polyethylene waxUsage: Michem® Shield 422 provides superior rub resistance in graphic arts applications.Information provided by Michelman® |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | Measured on 25% mass solution in toluene at 25°C; BMS 0380 |
Kraton® D1152 E (SBS) Liner Block Copolymer Description: Kraton D1152 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1160 E (SIS) Linear Triblock Copolymer Description: Kraton D1160 E is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from Europe in the physical form identified: D1160 ES .. |
|||
Brookfield Viscosity | 1000 cP @Temperature 25.0 °C |
1000 cP @Temperature 77.0 °F |
Toluene solution. Neat polymer concentration, 25%w. |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 54255 Multi-functional epoxy dispersion Description: Multi-functional epoxy dispersionUsage: Michem® Emulsion 54255 is a modified multi-functional epoxy dispersion which exhibits exceptional flexibility and toughness. It can be used fo.. |
|||
Brookfield Viscosity | <= 1000 cP | <= 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 72040 Nonionic polyethylene wax emulsion Description: Nonionic polyethylene wax emulsion Usage: Michem® Emulsion 72040 was designed to be an additive for the graphic arts industry and provides excellent rub, mar and scratch resistance.W.. |
|||
Brookfield Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/12 Polyester based TPU Pearlstick 46-10/12 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility:.. |
|||
Brookfield Viscosity | 1000 - 1600 cP @Temperature 25.0 °C |
1000 - 1600 cP @Temperature 77.0 °F |
10% solids aqueous solution, #3 spindle, Model LVF, 60 rpm |
DuPont Elvanol® 85-91 Polyvinyl Alcohol Specialty and Adhesive Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Brookfield Viscosity | 1000 cP @Temperature 160 °C |
1000 cP @Temperature 320 °F |
ETM E-31 |
ExxonMobil ESCOREZ™ 2184 (Europe) Petroleum Hydrocarbon Resin Aromatic modified aliphatic hydrocarbon resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It is especially useful as a single tackifier for natura.. |
|||
Brookfield Viscosity | 1000 - 1400 cP @Temperature 25.0 °C |
1000 - 1400 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 203 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 203: Polyester resin.. |
|||
Brookfield Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | Part A, CP#52 @ 100 rpm |
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg.. |
|||
Brookfield Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | Part A, CP #52 @ 100 rpm |
3M Scotch-Weld™ DP601 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Brookfield Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | Part A, CP #52 @ 100 rpm |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Brookfield Viscosity | 1000 cP | 1000 cP | Catalyst |
BCC Products BC 9040 T Silicone RTV Rubber BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high.. |
|||
Brookfield Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | RVT #3 sp @ 20 rpm |
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |