Polymer Property : Shear Strength = 1740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 12.0 MPa

@Temperature 22.0 °C,
Time 86400 sec
>= 1740 psi

@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
Palm Labs Adhesives TURBO-LOCK SERIES 17-ED Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-ED is a fast curing, YELLOW, medium strength, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly resistance to vibration..