This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.13 - 1.15 g/cc
0.0408 - 0.0415 lb/in³
Average value: 1.14 g/cc Grade Count:8
Moisture Vapor Transmission 2.18 - 7.38 cc-mm/m²-24hr-atm
5.54 - 18.7 cc-mil/100 in²-24hr-atm
Average value: 4.78 cc-mm/m²-24hr-atm Grade Count:4
0.230 - 0.340 cc-mm/m²-24hr-atm

@Temperature 38.0 - 38.0 °C
0.584 - 0.864 cc-mil/100 in²-24hr-atm

@Temperature 100 - 100 °F
Average value: 0.285 cc-mm/m²-24hr-atm Grade Count:2
Water Vapor Transmission 145 - 295 g/m²/day
9.34 - 19.0 g/100 in²/day
Average value: 220 g/m²/day Grade Count:4
9.00 - 9.00 g/m²/day

@Temperature 38.0 - 38.0 °C
0.580 - 0.580 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 9.00 g/m²/day Grade Count:2
Oxygen Transmission 0.190 - 3.60 cc-mm/m²-24hr-atm
0.483 - 9.14 cc-mil/100 in²-24hr-atm
Average value: 1.15 cc-mm/m²-24hr-atm Grade Count:7
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 50.0 - 370 %
50.0 - 370 %
Average value: 224 % Grade Count:7
Film Elongation at Break, TD 200 - 400 %
200 - 400 %
Average value: 286 % Grade Count:7
Secant Modulus, MD 0.620 - 2.26 GPa
89.9 - 328 ksi
Average value: 1.17 GPa Grade Count:7
Secant Modulus, TD 0.620 - 2.26 GPa
89.9 - 328 ksi
Average value: 1.12 GPa Grade Count:7
Charpy Impact Unnotched NB - NB

@Temperature -30.0 - -30.0 °C
NB - NB

@Temperature -22.0 - -22.0 °F
Grade Count:1
Charpy Impact, Notched 0.500 - 0.500 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 2.38 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.500 J/cm² Grade Count:1
Coefficient of Friction 0.450
0.450
Average value: 0.450 Grade Count:3
Elmendorf Tear Strength, MD 1.00 - 3.00 g/micron
25.4 - 76.2 g/mil
Average value: 1.86 g/micron Grade Count:7
Elmendorf Tear Strength, TD 0.800 - 5.00 g/micron
20.3 - 127 g/mil
Average value: 2.37 g/micron Grade Count:7
Dart Drop Test 400 - 600 g
0.882 - 1.32 lb
Average value: 550 g Grade Count:4
Film Tensile Strength at Break, MD 52.0 - 240 MPa
7540 - 34800 psi
Average value: 115 MPa Grade Count:7
Film Tensile Strength at Break, TD 17.0 - 76.0 MPa
2470 - 11000 psi
Average value: 50.7 MPa Grade Count:7
Optical Properties Metric English Comments
Haze 0.500 - 8.00 %
0.500 - 8.00 %
Average value: 2.36 % Grade Count:7
Gloss 65.0 - 150 %
65.0 - 150 %
Average value: 136 % Grade Count:7