Polymer Property : Moisture Vapor Transmission = 7.38 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 2.18 - 7.38 cc-mm/m²-24hr-atm
5.54 - 18.7 cc-mil/100 in²-24hr-atm
Average value: 4.78 cc-mm/m²-24hr-atm Grade Count:4
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..