Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.230 - 0.340 cc-mm/m²-24hr-atm @Temperature 38.0 - 38.0 °C |
0.584 - 0.864 cc-mil/100 in²-24hr-atm @Temperature 100 - 100 °F |
Average value: 0.285 cc-mm/m²-24hr-atm Grade Count:2 |