Polymer Property : Elmendorf Tear Strength, TD = 127 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 0.800 - 5.00 g/micron
20.3 - 127 g/mil
Average value: 2.37 g/micron Grade Count:7
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..