Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 52.0 - 240 MPa
7540 - 34800 psi
Average value: 115 MPa Grade Count:7
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..