Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman PE 1011 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman PE1055 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman PE1080 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman PE1257 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through .. |
|||
Film Tensile Strength at Break, TD | 17.0 - 66.2 MPa | 2470 - 9600 psi | Average value: 36.8 MPa Grade Count:18 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou.. |
|||
Film Tensile Strength at Break, TD | 17.0 - 76.0 MPa | 2470 - 11000 psi | Average value: 50.7 MPa Grade Count:7 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | Cast; ASTM D822 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | Cast; ASTM D822 |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Braskem BC 818 LDPE Extrusion Coating Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Extrusion coating. Information provided by Braskem |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose. Information provided by Braskem |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ISO 1184 |
Carmel Olefins IPETHENE® 111 Low Density Polyethylene IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ISO 1184 |
Carmel Olefins IPETHENE® 113 Low Density Polyethylene IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin.. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Film Tensile Strength at Break, TD | 17.0 - 17.9 MPa | 2470 - 2600 psi | Average value: 17.3 MPa Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Film Tensile Strength at Break, TD | 17.0 MPa | 2470 psi | ASTM D882 |
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con.. |