Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman PE 1011 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman PE1055 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman PE1080 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman PE1257 EVA Film Extrusion  (discontinued **)
2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman PE 1302 EVA Film Extrusion  (discontinued **)
3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through ..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through ..
Film Tensile Strength at Break, TD 17.0 - 66.2 MPa
2470 - 9600 psi
Average value: 36.8 MPa Grade Count:18
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou..
Film Tensile Strength at Break, TD 17.0 - 76.0 MPa
2470 - 11000 psi
Average value: 50.7 MPa Grade Count:7
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
Cast; ASTM D822
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
Cast; ASTM D822
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film
Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer
Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Braskem BC 818 LDPE Extrusion Coating Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Extrusion coating. Information provided by Braskem
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose. Information provided by Braskem
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ISO 1184
Carmel Olefins IPETHENE® 111 Low Density Polyethylene
IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ISO 1184
Carmel Olefins IPETHENE® 113 Low Density Polyethylene
IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin..
Film Tensile Strength at Break, TD 17.0 - 17.9 MPa
2470 - 2600 psi
Average value: 17.3 MPa Grade Count:3
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..
Film Tensile Strength at Break, TD 17.0 MPa
2470 psi
ASTM D882
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con..
Copyright © lookpolymers.com All Rights Reserved