NYCOA 715C PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 715C PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
plasticized, high viscosity extrusion grade for monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 3.1 %
3.1 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 0.862 GPa
125 ksi
ASTM D790
Izod Impact, Notched 16.63 J/cm
31.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 220 °C
428 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F