Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
NYCOA 715C PA 6 plasticized, high viscosity extrusion grade for monofilament weed eater, fishing lineInformation provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MK0049A PP (Europe-Africa-Middle East) LNP* STARFLAM* MK0049A is a compound based on Polypropylene resin containing Talc, Flame Retardant. Added features include : Flame Retardant. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology 40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Tipco Tipcolene® DR 8201 - 20% Talc/Mineral Reinforced, Impact Modified, Polypropylene Copolymer 20% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Tipco Tipcolene® FPC 40 PPC - 40% Calcium Carbonate Reinforced Polypropylene Copolymer 40% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified An extrusion grade nylon 6 copolymer that provides excellent melt strength, impact, tensile elongation and flexibility.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 37.0 MPa | 5370 psi | DIN 53452 |
Ineos Nova S-3207 Medium Impact Compact Polystyrene
(discontinued **) High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A.. |