Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.2 MPa
3950 psi
ASTM D638
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D638
Elongation at Break 1500 %
1500 %
ASTM D638
Elongation at Yield 17.4 %
17.4 %
ASTM D638
Flexural Modulus 0.610 GPa
88.5 ksi
ASTM D790
Izod Impact, Notched 5.30 J/cm

@Thickness 3.20 mm
9.93 ft-lb/in

@Thickness 0.126 in
ASTM D256
Tensile Impact Strength 163 kJ/m²
77.6 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
ASTM D3417
Crystallization Temperature 112 °C
234 °F
ASTM D3417
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D1525
Vicat Softening Point 113 °C
235 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 204 - 315 °C
399 - 599 °F
Copyright © lookpolymers.com All Rights Reserved