Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
9.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Nylene® PA6 Impact Modified 323 HS Nylon 6 Extrusion Grade; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | |
Spartech Spectrum® S370 TPO Polyolefin Sheet
(discontinued **) Data provided by the manufacturer. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Rostone Rosite® 4010ES SMC Thermoset Polyester, 22-25% Glass Reinforced
(discontinued **) Key Features: Business Machine GradeHigh strength, dimensional control, and surface smoothness.Information provided by Oneida-Rostone Group. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D 256 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals .. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256A |
LyondellBasell Astryn BA16G Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weath.. |
|||
Izod Impact, Notched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.20 mm |
9.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.20 mm |
9.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® T 45 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P114 PBT Polyester A high impact polyester with low shrinkage.Data provided by the manufacturer |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.17 mm |
9.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.20 mm |
9.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |