Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.30 J/cm @Temperature -10.0 °C |
9.93 ft-lb/in @Temperature 14.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
9.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Nylene® PA6 Impact Modified 323 HS Nylon 6 Extrusion Grade; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Izod Impact, Notched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Izod Impact, Notched | 5.30 - 5.30 J/cm @Temperature -10.0 - -10.0 °C |
9.93 - 9.93 ft-lb/in @Temperature 14.0 - 14.0 °F |
Average value: 2.37 J/cm Grade Count:1 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 5.30 - 7.50 J/cm | 9.93 - 14.1 ft-lb/in | Average value: 6.57 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Rostone Rosite® 4010ES SMC Thermoset Polyester, 22-25% Glass Reinforced
(discontinued **) Key Features: Business Machine GradeHigh strength, dimensional control, and surface smoothness.Information provided by Oneida-Rostone Group. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals .. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256A |
LyondellBasell Astryn BA16G Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weath.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256A |
LyondellBasell Astryn SB572C Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, extrusion grade polypropylene copolymer, good melt strength, good processabilityApplications: solar panelsDescription: Astryn SB572C fractional me.. |
|||
Izod Impact, Notched | 5.30 J/cm @Temperature 23.0 °C |
9.93 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 5.30 J/cm @Temperature -30.0 °C |
9.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.20 mm |
9.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Izod Impact, Notched | 5.30 J/cm | 9.93 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Izod Impact, Notched | 5.30 J/cm @Thickness 3.20 mm |
9.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |