Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.2 MPa | 3950 psi | ASTM D638 |
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 27.2 MPa | 3950 psi | |
3M Jet-Weld™ TE-015 Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.Extrudable. Very fast set time for bonding wood and selected plasticsInformation pro.. |
|||
Tensile Strength, Ultimate | 27.2 MPa | 3950 psi | ASTM D638 |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 27.3 MPa | 3950 psi | |
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |