Polymer Property : Tensile Strength, Yield = 2510 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D412
Precision Polymer Engineering Z95Z Hydrogenated NBR Compound
Peroxide cured and methacrylate modified, hydrogenated nitrile rubber, 80-92 °IRHD. Medium acrylonitrile content (ACN=36%). ASTM designation = HNBR.Applications: For uses where very high physical ..
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D638
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals..
Tensile Strength, Yield 17.3 MPa
2510 psi
2 in/min, Type 1; ASTM D638
Solvay Engineered Polymers DEXFLEX® 711-300 TPO  (discontinued **)
Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color match..
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D638
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Tensile Strength, Yield 17.3 MPa
2510 psi
2"/min; ASTM D638
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA594189 is a pelletized LLDPE copolymer resin for injection molding thin-walled items requiring high flow and short cycle times. GA594189 exhibits excellent flow, warp resistance and sur..
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D638
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.