Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 163 kJ/m² | 77.6 ft-lb/in² | ASTM D1822 |
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Impact Strength | 163 kJ/m² | 77.6 ft-lb/in² | 0.3 cm notched sample; ASTM D1822 |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |