NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applications such as medium and high voltage cross-linked coatings and sheaths.LF-0222-A contains minimal antioxidant levels and therefore must be supplemental as required by Industry Specifications for the intended product.Information provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
Pellet; ASTM D792
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 49
49
ASTM D2240
Tensile Strength, Ultimate 9.70 MPa
1410 psi
ASTM D638
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Secant Modulus 0.193 GPa
28.0 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
NOVA
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Dielectric Constant 2.28

@Frequency 1e+6 Hz
2.28

@Frequency 1e+6 Hz
ASTM D1531
Dissipation Factor 0.00010

@Frequency 1e+6 Hz
0.00010

@Frequency 1e+6 Hz
ASTM D1531