Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® MQ B0 Very Low Density Polyethylene Clearflex MQ B0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity... |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® MS 40 U Linear Low Density Polyethylene Flexirene MS 40 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 40 U are characterized by a good balance be.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | F<sub>0</sub> notched specimen; ASTM D746 |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D 746 |
NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin 31G complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 31G is su.. |
|||
Brittleness Temperature | -70.0 - -35.0 °C | -94.0 - -31.0 °F | Average value: -67.0 °C Grade Count:25 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin
(discontinued **) Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufactu.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 59F HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 96A-UV8D HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free, excellent UV resistance.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial or.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil HD 6908.18 Injection Molding Resin
(discontinued **) HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D746 |
Lushan L-5R Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding Key Characteristics:Good flowability for multicavitiesGood toughness and flexibilityExcellent gloss and transparencyOdorlessSafe for food contactRecommended Applications:HousewaresSmall to large clo.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H2040 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Like H4040, except that heat-ageing resistance is improved. Applications requiring better heat-ageing resistanc.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE) Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent tear resistance. Molded and injected products for consumer use, such as airbag door covers, railwa.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Good melt stability. CVJ boots, dust cover, bellows, jackets and .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | Average value: -70.0 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |